BÖHLER P848

BÖHLER P848 is an iron-48% -nickel alloy with low thermal expansion for applications in the electronics industry, for measuring instruments (e.g. measuring rulers, scales), temperature measuring instruments and temperature-dependent controls, thermostats, thermobimetals and expansion controllers up to temperatures of 450°C. The main application is in glass-metal compounds with soft lead crystal and soda-lime glasses.
The minimum coefficient of thermal expansion of BÖHLER P848 is in the range of 30 to 400°C. Above the break point at slightly above 450°C, the coefficient of expansion increases sharply and at higher temperatures reaches the values usual for austenitic materials. Good low temperature properties.

Formas de productos disponibles

Ruta de fusión

Aire fundido

Números de materiales

Market grade
Ni 48
SEL
1.3922
EN
Ni48

Estándares

Others
SEW 385

Chemical Composition

* Composición química (% promedio)

C
max. 0.05
Si
max. 0.30
Mn
max. 0.50
Ni
min. 46.0

Aplicaciones