BÖHLER A959

BÖHLER A959 (Alloy 28, UNS N08028, W. Nr. 1.4563) is a nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as pitting and crevice corrosion. The alloy is especially resistant to sulphuric and phosphoric acid. Equipment used for chemical processing, pollution control equipment, oil and gas well piping ,natural gas and oil transportation, nuclear fuel reprocessing and transportation, acid production and pickling equipment and transportation
The alloy was originally developed for use in the manufacture of phosphoric acid, especially for heat exchangers in the concentration unit, where corrosive conditions are at their worst.

Formas de productos disponibles

Productos largos: Los datos presentados se refieren exclusivamente a productos largos. Consulte las explicaciones detalladas al final de la ficha técnica (pdf).

Ruta de fusión

Aire fundido

Números de materiales

Market grade
Alloy 28
SEL
1.4563
EN
X1NiCrMoCu31-27-4
UNS
N08028

Estándares

EN ISO
10088-3

Chemical Composition

* Composición química (% promedio)

C
max. 0.020
Si
max. 0.70
Mn
max. 2.00
P
max. 0.030
S
max. 0.010
Cr
26.0 to 28.0
Mo
3.0 to 4.0
Ni
30.0 to 32.0
Cu
0.70 to 1.50
N
max. 0.10

Aplicaciones